Cellulose oxidative and hydrolytic degradation: In situ FTIR approach J £ojewska, P Mi¶kowiec, T £ojewski, LM Proniewicz Polymer degradation and stability 88 (3), 512-520, 2005 | 478 | 2005 |
Degradation markers of fibroin in silk through infrared spectroscopy MA Koperska, D Pawcenis, J Bagniuk, MM Zaitz, M Missori, T £ojewski, ... Polymer Degradation and Stability 105, 185-196, 2014 | 119 | 2014 |
FTIR and UV/vis as methods for evaluation of oxidative degradation of model paper: DFT approach for carbonyl vibrations T £ojewski, P Mi¶kowiec, M Missori, A Lubañska, LM Proniewicz, ... Carbohydrate Polymers 82 (2), 370-375, 2010 | 95 | 2010 |
Evaluating paper degradation progress. Cross-linking between chromatographic, spectroscopic and chemical results T £ojewski, K Ziêba, A Knapik, J Bagniuk, A Lubañska, J £ojewska Applied Physics A 100, 809-821, 2010 | 89 | 2010 |
Heat Treatment Effect on Crystalline Structure and Photoelectrochemical Properties of Anodic TiO2 Nanotube Arrays Formed in Ethylene Glycol and Glycerol … M Jarosz, K Syrek, J Kapusta-Ko³odziej, J Mech, K Ma³ek, K Hnida, ... The Journal of Physical Chemistry C 119 (42), 24182-24191, 2015 | 81 | 2015 |
FTIR in situ transmission studies on the kinetics of paper degradation via hydrolytic and oxidative reaction paths J £ojewska, A Lubañska, P Mi¶kowiec, T £ojewski, LM Proniewicz Applied Physics A 83, 597-603, 2006 | 78 | 2006 |
Size exclusion chromatography and viscometry in paper degradation studies. New Mark-Houwink coefficients for cellulose in cupri-ethylenediamine T £ojewski, K Ziêba, J £ojewska Journal of Chromatography A 1217 (42), 6462-6468, 2010 | 63 | 2010 |
Structured cobalt oxide catalyst for VOC combustion. Part I: Catalytic and engineering correlations J £ojewska, A Ko³odziej, T £ojewski, R Kapica, J Tyczkowski Applied Catalysis A: General 366 (1), 206-211, 2009 | 58 | 2009 |
High aspect-ratio semiconducting ZnO nanowires formed by anodic oxidation of Zn foil and thermal treatment L Zaraska, K Mika, KE Hnida, M Gajewska, T £ojewski, M Jasku³a, ... Materials Science and Engineering: B 226, 94-98, 2017 | 52 | 2017 |
Vibrational spectroscopy to study degradation of natural dyes. Assessment of oxygen-free cassette for safe exposition of artefacts M Koperska, T £ojewski, J £ojewska Analytical and bioanalytical chemistry 399, 3271-3283, 2011 | 48 | 2011 |
Furfural as a marker of cellulose degradation. A quantitative approach T £ojewski, T Sawoszczuk, JM £agan, K Ziêba, A Barañski, J £ojewska Applied Physics A 100, 873-884, 2010 | 48 | 2010 |
Spectroscopic characterization of Co3O4 catalyst doped with CeO2 and PdO for methane catalytic combustion PJ Jod³owski, RJ Jêdrzejczyk, A Rogulska, A Wach, P Ku¶trowski, ... Spectrochimica Acta Part A: Molecular and Biomolecular Spectroscopy 131, 696-701, 2014 | 39 | 2014 |
Application of computational intelligence methods for the automated identification of paper-ink samples based on LIBS K Rzecki, T So¶nicki, M Baran, M Nied¼wiecki, M Król, T £ojewski, ... Sensors 18 (11), 3670, 2018 | 38 | 2018 |
Acid-catalysed degradation A Barañski, JM £agan, T £ojewski Ljubljana: National and University Library, 2005 | 33 | 2005 |
On the use of ASTM closed vessel tests in accelerated ageing research T Sawoszczuk, A Barañski, JM £agan, T £ojewski, K Ziêba Journal of cultural heritage 9 (4), 401-411, 2008 | 32 | 2008 |
Nanoporous tin oxides synthesized via electrochemical anodization in oxalic acid and their photoelectrochemical activity L Zaraska, K Syrek, KE Hnida, M Bobruk, A Krzysik, T £ojewski, M Jasku³a, ... Electrochimica Acta 205, 273-280, 2016 | 30 | 2016 |
Evaluating degradation of silk’s fibroin by attenuated total reflectance infrared spectroscopy: Case study of ancient banners from Polish collections MA Koperska, T £ojewski, J £ojewska Spectrochimica Acta Part A: Molecular and Biomolecular Spectroscopy 135, 576-582, 2015 | 30 | 2015 |
Kinetic approach to degradation of paper. In situ FTIR transmission studies on hydrolysis and oxidation J £ojewska, A Lubañska, T £ojewski, P Mi¶kowiec, LM Proniewicz e-Preservation Science 2, 1-11, 2005 | 30 | 2005 |
Activation and deactivation of cobalt catalysts in the hydrogenation of carbon dioxide G Fröhlich, U Kestel, J £ojewska, T £ojewski, G Meyer, M Voß, ... Applied Catalysis A: General 134 (1), 1-19, 1996 | 30 | 1996 |
An experimental study of the pressure drop in fluid flows through wire gauzes A Ko³odziej, M Jaroszyñski, B Janus, T Kleszcz, J £ojewska, T £ojewski Chemical Engineering Communications 196 (8), 932-949, 2009 | 28 | 2009 |